杏彩平台

Jacket compound EM2

NO.

Test Items

Values

1

Before ageing test

1.1 Tensile strength(MPa)

≥10.0

1.2 Elongation at break(%)

≥300

2

After oven ageing test

2.1 Test condition80±2℃/240h

2.2 Tensile strength rate(%)

±15
2.3 Elongation at break rate(%)±15
3Oil-resistance test(IRM902 oil)3.1 Test condition100±2℃/240h
3.2 Tensile strength rate(%)±40
3.3 Elongation at break rate(%)±40
4Ozone ageing test4.1 Test condition40℃/72h, concentration 2ppm or 25℃/24h, 260ppm
4.2 Test resultWithout crack
5

Heat extension test

5.1 Test condition

200±3℃/15min, stress 20N/cm2

5.2 Loading elongation rate(%)< 100
5.3 Loaded elongation rate(%)< 25
6Low-temperature impact test6.1 Test condition-40℃/4h
6.2 Wire surface after low-temperature impactWithout crack
7Oxygen index and flame resistance (EN50265-2-1 burning test)≥32
Standard No.:GB5013 & HD22 & VDE282